LiNiCoMnO2 (Lithium Nickel Manganese Cobalt Oxide) powder for Li-ion power battery cathode 200g/bottle (Ni:Co:Mn=5:2:3, NCM523 or NMC532)Specification Item Description Testing Method D10 (μm) ≤ 5.0 Laser Particle Size Analyzer D50 (μm) 10.0-14.0 D90 (μm) ≥25.0 Appearance Dark brown powder, atmospheric stability Elements Proportions Ni:Co:Mn = 5:2:3 Ni+Co+Mn (%) ≥58 Volumetry Li (%) 7.00-8.00 Atomic Absorption SpectroscopyInductively Coupled Plasma Fe (%) ≤0.01 Na (%) ≤0.03 Cu (%) ≤0.005 H2O (%) ≤0.05 Coulometric KF Titrator PH ≤ 11.50 PH Tester H2O (%) ≤ 0.1 Moisture Analyzer Specific Surface Area (m2/g) 0.20-0.40 BET Analyzer Specific Capacity (mAh/g) [1st cycle] 153-158 0.2C, 4.2-2.7 V vs Li/Li+, Half Cell Columbia Efficiency (%) [1st cycle] ≥85% Note: MTI does not manufacture this product, and only sell the small quantity to research for development for new generation battery. If you need a larger quantity or have the question for IP, we will forward your inquiry to the producer. XRD SEM Particle Size Application Notes: Please click to see Procedure for Preparing Anode & Cathode Electrode Slurry. Please keep the powder in vacuum box to avoid moisture. Please bake the powder in a vacuum oven at 120 - 150 °C before making slurry and coating to ensure max. capacity. Related Products Vacuum Storage Box Powder Milling & Mixer Electrode Coaters Battery Research Equipment Other Battery Powders