PVDF (Polyvinylidene fluoride ) binder (particle size = ~ 30 um) is for mixing together with cathode or anode powder to prepare Li-ion battery electrode 80g/bag, vacuum sealed in the a plastic bag SPECIFICATIONS: Technical Parameter Unit Index Testing Shape / White Powder / Purity % ≥99.5 PVDF standard specific gravity / 1.74~1.77 ASTM D 792 @23/23 Dielectric constant 100MHz100Hz 4.50~5.50 8.00~9.50 ASTM D150 Melting Point 160-168 ASTM D 3418 Melting Index g/10min 1-2 / Solubility / Transparent and dissolvable 301hr 1g/10ml NMP Rotation Viscosity mPa·S ≥2000 1g/10ml NMP30 Intrinsic Viscosity dL/g 1.0-2.0 DMA30 Moisture % ≤ 0.1 Karl Fischer Molecular Weight / 600,000 ASTM D 5296-05 Application Notes: Please click to see Step by Step Recipe for Preparing Anode & Cathode Electrode Slurry Note: PVDF resins have good thermostability at the temperature below 310. However, it will decompose into the toxic hydrogen fluoride and fluorocarbon. If it is idle for a long time at the temperature between 310 and 320. It is not suggested to use PVDF resin at temperature higher than 370 because this will accelerate the decomposition velocity in suchan environment. Besides, please keep in mind that PVDF resin will release toxic hydrogen fluoride and fluorocarbon when it burns.